PhthalocyaninePraseodymium Bio atomic_steps Piezoresponse Gallium_Arsenide non_contact LiquidImaging mono_layer Grain Plug Sulfur PDMS PatternedSapphireSubstrat Sperm Alkane SThM 2dMaterials LifeScience FM_SKPM MoirePattern LightEmission Organic DeflectionOptics PyroelectricDetector ScanningSpreadingResistanceMicroscopy Crystal organic_polymer ForceVolumeImage Bmp ConductingPolymer NUS_Physics MagneticPhase Varistor Heating OxideLayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polycrystalline ferroelectric BCZT
Scanning Conditions
- System: NX12
- Scan Mode: PFM
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.4Hz
- Pixel: 256×256
- Sample bias sweep range for Piezoresponse curve: -10V ~ +10V