Nanostructure align Materials CopperFoil Boundary Neodymium Granada OxideLayer neodymium_magnets MultiferroicMaterials Varistor ShenYang Copolymer AlkaneFilm MembraneFilter Tapping Annealing Beads dielectric trench Electical&Electronics semifluorinated_alkanes Regensburg Sulfur Yeditepe_University LithiumNiobate ContactMode TemperatureControl PvdfBead Etch Gallium_Arsenide alkanes Aggregated_molecules Polypropylene FailureAnlaysis StyreneBeads
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PVDF beads
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: Arrow UHF (f=2000kHz)
- Scan Size: 30μm×30μm, 10μm×10μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: Arrow UHF (f=2000kHz)
- Scan Size: 30μm×30μm, 10μm×10μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 512×512, 512×512