Worcester_Polytechnic_Institute ForceVolumeMapping SKPM ItoGlass OpticalWaveguide Vac phase_change Polystyrene Heat Tungsten_disulfide HexagonalBN C60H122 SoftSample Formamidinium_lead_iodide Hexatriacontane Magnets Heating Vortex Strontium VinylAlcohol Boundary MetalCompound #Materials ConductiveAFM Gold silicon_oxide Cancer Piezoelectric Ito Inorganic PhaseChange IVSpectroscopy CuParticle Optic mono_layer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: ElectriMulti75 (k=3 N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256