Wonseok TipBiasMode LightEmission Laser Trench MfmAmplitude Global_Comm TemperatureControl pulsed_laser_deposition temp OpticalModulator Sapphire LifeScience LiquidImaging SoftSample Wang molecular_beam BloodCell Spain PiezoelectricForceMicroscopy SrTiO3 Mfm SingleCrystal LiquidCell Beads Cobalt-dopedIronOxide UnivCollegeLondon Non-ContactMode PpLdpe NUSNNI PhaseTransition Fluoride thermal_property FAPbI3 InorganicCompound
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V