frequency_modulation Polyurethane dichalcogenide Regensburg Chromium Platinum Fujian ThermalDetectors thermal_conductivity Annealing Spain CrossSection Indium_tin_oxide PetruPoni OpticalModulator BFO CNT mono_layer CompactDisk Electrode SiliconCrystal NiFe SmallScan HexagonalBoronNitride Vac Sic Implant Phthalocyanine Chemical_Vapor_Deposition Hydroxyapatite Sadowski SingleCrystal PpLdpe Ceramic cross section
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li stripping-plating on Li surface
Scanning Conditions
- System : NX10 in dry room
- Scan Mode: Contact/EC AFM
- Scan Rate : 0.15 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : Multi75-G
- ECr : Li metal (Working electrode), Li metal (Reference electrode), Li (Counter electrode), 1M LiTFSI in TEGDME (Electrolyte)
- Open circuit voltage : 1 VLi/Li+