Electical&Electronics NanoLithography nanomechanical Optoelectonics Litho Conducting Inorganic_Compound HafniumDioxide Croatia Ecoli SurfaceChange Ferroelectric MagneticPhase HardDiskMedia BiFeO3 Ito Piezo PrCurve YszSubstrate MechanicalProperties Kevlar Dimethicone OpticalModulator MagneticForce Hole Calcium PtfeFilter INSPParis LaAlO3 fluoroaalkane AmplitudeModulation Magnetic Force Microscopy FailureAnlaysis tip_bias_mode Memory
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Imprint sample
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256