StyreneBeads Dopped bias_mode Liquid Insulator Workfunction Sapphire LiBattery Ni81Fe19 Vortex Hexatriacontane Piezo HiVacuum neodymium_magnets Anneal cooling piezoelectric force microscopy OrganicCompound PS_PVAC Vinylpyridine DeflectionOptics DOE #EC Mechanical&nanotechnology Yttria_stabilized_Zirconia Fujian ItoGlass solar_cell Electrode Deposition Mosfet PhaseImaging Organic UnivCollegeLondon NanoLithography
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcite surface change in Ca(OH)2
Scanning Conditions
- System: NX20
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256