Optoelectonics PvdfFilm HACrystal Melt MolecularSelfAssembly HBN Cell SoftSample Formamidinium_lead_iodide SrTiO3 Barium_titanate 2d_materials Cancer Phthalocyanine rubber BCZT blended polymers LiNbO3 atomic_steps IRDetector Annealing Conductance cannabis Conducting ForceDistanceSpectroscopy Growing Trench CancerCell AdhesionEnergy Morphology Strontium Nanotechnology Tungsten graphene_hybrid BismuthVanadate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BFO (BiFeO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 5μm×5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512