DNA Hysteresys aluminum_nitride IIT-chennai Polyethylene Lift LateralPFM GranadaUniv rubber Lateral_Force_Microscopy Lateral suspended_graphene AdhesionEnergy HighResolution OpticalElement Vac I-VSpectroscopy Semiconductor lift_mode Polyaniline Solar ScanningSpreadingResistanceMicroscopy Foil NUS_Physics KelvinProbeForceMicroscopy LiftHeight Gold ShenYang cooling UnivMaryland Indium_tin_oxide MBE semifluorinated alkane thermal_conductivity Protein
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer Ι
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512