India AEAPDES ForceDistanceSpectroscopy MolecularSelfAssembly LithiumNiobate Scratch Ananth mechanical property Al2O3 UTEM SiliconOxide blended polymers Gold SKPM SrO piezoelectric force microscopy aluminum_nitride Force-distance CarbonNanotube Annealing Monisha BismuthVanadate PolyStylene STO Optoelectronic PinpointNanomechanicalMode Pattern Perovskite HOPG Pinpoint TransitionMetal TungstenDeposition mechanical_property solar_cell Korea
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cannabidiol(CBD) Molecules
CBD(concentration: 20 mg/mL) molecules assembled on Mica surface after solution rinsing Aggregated CBD molecules as a ring shape.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256