#Materials Dimethicone HexagonalBN fluoroaalkane Chemical_Vapor_Deposition Vanadate Pore MBE CNT LMF PhthalocyaninePraseodymium DeoxyribonucleicAcid Au111 Hexatriacontane TriGlycineSulphate WS2 Boundary FM_KPFM suspended_graphene SmallScan Yttria_stabilized_Zirconia GalliumPhosphide AmplitudeModulation AdhesionEnergy PhaseChange exfoliate Barium_titanate Polymer Gallium ElectroDeposition MESA structure India Optoelectronic Domain Adhesive
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cutting Graphene
Scanning Conditions
- System : FX40
- Scan Mode: Contact after lithography
- Scan Rate : 0.7 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)
- Lithography condition : Force 500 nN, writing speed 0.1μm/s, AC bias 10 V @ 40kHz