Cross-section TemperatureControlledAFM ContactMode VortexCore ferromagnetic CarbonNanotube Granada Piezo ElectroChemical Cell organic_polymer ULCA CuFoil temperature_control Tapping WS2 Pore TransitionMetal Hair INSPParis Change BiasMode Kevlar Water LFM SingleCrystal nanobar light_emission Scratch MagneticArray Chungnam_National_University Forevision OrganicSemiconductor Biofilm Lift
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V