hard_disk_media Pore IndiumTinOxide PhaseImaging DOE MoS2 SKKU Cobalt-dopedIronOxide FM_KPFM Ca10(PO4)6(OH)2 Solution Thermoplastic_polyurethane YttriaStabilizedZirconia hetero_structure bias_mode BiFeO3 DNA Inorganic BiVO4 Conductance rubber TemperatureControllerAFM LowDensityPolyethylene Epoxy Crystal CuFoil Solar self-assembly LDPE cooling polymeric_arrays PinPointMode Aluminum Aluminium_Oxide FrictionalForce
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Imprint sample
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256