India MeltingPoint Battery aluminum_nitride Plug medical IIT-chennai Cross-section temperature controller AFM AdhesionEnergy Mfm MembraneFilter TungstenThinFilmDeposition Self-assembledMonolayer Modulus LightEmission FailureAnlaysis Conductance InorganicCompound Chungnam_National_University China CalciumHydroxyapatite Growing Composition NCM\ Optic Oxidation Crystal SPMLabs Ito Singapore Copper Non-ContactMode PS_PVAC LiftMode
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Perovskite
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36A Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 4μm×4μm
- Scan Rate: 0.3Hz
- Pixel: 512×256