hydrocarbon IMT_Bucharest EFMAmplitude ContactModeDots Inorganic Molybdenum HexagonalBN Tape Ferroelectric LifeScience PvdfBead blended polymers MagneticForce I-VSpectroscopy Piezoelectric MultiferroicMaterials HACrystal IIT-chennai Al2O3 PolyimideFilm heterojunctions WS2 Mapping graphene_hybrid BariumTitanate CrossSection TPU CuSubstrate Foil Insulator OpticalWaveguides PDMS PUR Switching pulsed_laser_deposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Al2O3-doped CaMnO3
1% Al2O3-doped CaMnO3 on LaAlO3 (001) orientation substrate by pulsed laser deposition.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256