C60H122 AdhesionForce pinpoint mode exfoliate Polyaniline GranadaUniv Foil atomic_steps SurfaceOxidation NanoLithography SKKU Solution hetero_structure ElectroDeposition Heating Flake Croatia AAO MonoLayer Mapping Bmp Cross-section BiasMode SThM IMT_Bucharest gallium_nitride DIWafer Materials HiVacuum ForceVolumeImage TungstenDeposition ChemicalCompound Sulfur Sperm Adhesion
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ER 316L Stainless Steel
The ferrite MFM phase has a striped appearance due to its ferromagnetic behavior, while the paramagnetic austenite phase shows a uniform appearance.
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm