Boundary LithiumNiobate Nickel Glass 3-hexylthiophene Pattern Film Hexatriacontane Domain graphene_hybrid Yeditepe UnivOfMaryland HardDisk Techcomp dielectric_trench SolarCell SingleLayer norganic ItoGlass Fendb Metal-organicComplex Liquid pulsed_laser_deposition Temasek_Lab StrontiumTitanate MultiLayerCeramicCapacitor VortexCore dielectric trench VinylAlcohol electrospinning SrO Crystal Pvdf MoirePattern Gold
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
C36H74
Layer of C36H74 alkane on HOPG.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256