Ananth non_contact HOPG dielectric_trench OrganicSemiconductor WPlug doped Blood epitaxy PFM HighAcpectRatio Polyurethane CntFilm Polystyrene Dental SrO Austenite cannabis suspended_graphene Aluminium_Oxide SicMosfet Ca10(PO4)6(OH)2 Molybdenum NUS_NNI_Nanocore Non-ContactMode PolymerPatterns BCZT HafniumDioxide Cancer PS_LDPE Vanadate frequency_modulation Pvdf Mobile AdhesionEnergy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PP/LDPE polymer blend
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint mechanical
- Cantilever: FMR (k=2N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.35Hz
- Pixel: 256×256
- Modulus calculation model: Hertzian