ElectroChemical KevlarFiber PinpointPFM NeodymiumMagnets PMNPT hard_disk_media high_resolution Ptfe SThM PinPointMode BismuthFerrite Microchannel layers CuFoil FrictionalForceMicroscopy KPFM IRDetector 2d_materials Magnetostrictive FAPbI3 2dMaterials Fujian strontiu_titanate FM_SKPM TemperatureControllerStage HexagonalBoronNitride Indium_tin_oxide BFO thermoplastic_elastomers PiezoelectricForceMicroscopy Calcite DIWafer Piranha Conductive AFM HumanHair
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hard defect repair of photomask
Scanning Conditions
- System : NX-Mask
- Scan Mode: Non-contact for imaging Sweep for repairing
- Scan Rate : 0.3 Hz
- Scan Size : 1.25μm×1.25μm
- Pixel Size : 256×256
- Cantilever : OMCL-AC160TS for imaging, AD-40 AS for repairing (k=42N/m, f=330kHz)