AlkaneFilm Mapping Alkane AdhesionForce C60H122 Morphology lithography HardDiskMedia Gallium INSPParis PVA Writing Semiconductor Metal Gold Glass SmallScan Chemical_Vapor_Deposition Perovskite Domain TungstenDeposition IISCBangalore norganic BismuthVanadate PDMS TappingMode Defect Molybdenum_disulfide Electronics Spain OpticalElement FailureAnalysis hetero_structure Ni-FeAlloy plastic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ceramic Portland cement
Scanning Conditions
- System : NX10
- Scan Mode: Tapping
- Scan Rate : 1Hz
- Scan Size : 1μm×1μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)