self-assembled_monolayer Growth PetruPoni_Institute food Chloroform Battery 2d_materials Defect Phosphide Corrosion ScanningThermalMicroscopy Pipette Yttria_stabilized_Zirconia Deposition Lattice Nickel atomic_layer temperature_control CuFoil doped Metal-organicComplex Heat Steps WWafer VortexCore PolycrystallineFerroelectricBCZT medical Sperm EPFL Melt IMT_Bucharest strontiu_titanate BariumTitanate STO Hysteresys
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Scanning Conditions
- System : FX40
- Scan Mode: PinPoint nanomechanical
- Scan Rate : 0.15 Hz
- Scan Size : 50μm×50μm
- Pixel Size : 256×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)