Sic epitaxy BiasMode PECurve ForceVolumeImage high_resolution Treatment Flake OpticalElement MfmPhase SKKU CeramicCapacitor Phosphide MagneticForceMicroscopy NiFe Collagen NCM TPU Ca10(PO4)6(OH)2 Litho Fujian SolarCell cannabinoid WPlug semifluorinated_alkanes MetalCompound Adhesion electrospinning fluorocarbon ReflexLens Christmas LiNbO3 Mapping GaN Thermal
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V