plastics Mapping high_resolution Tin sulfide CaMnO3 amplitude_modulation Christmas ULCA Permalloy lithography LowDensityPolyethylene PMNPT PpLdpe hydrocarbon ScanningSpreadingResistanceMicroscopy Ferroelectric Composition KPFM Adhesive NtuEee Gold BCZT Ni81Fe19 CarbonNanotube ForceDistanceSpectroscopy Molybdenum_disulfide Temasek_Lab SFAs Lateral_Force_Microscopy Polytetrafluoroethylene align KevlarFiber BloodCell Ram StrontiuTitanate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256