Sidewall SrTiO3 Worcester_Polytechnic_Institute NiFe Jason Aggregated_molecules Typhimurium OpticalWaveguide TriGlycineSulphate Dr.JurekSadowski Spincast MechanicalProperty piezoelectric force microscopy contact LaAlO3 Conductance Etch Growth DomainSwitching AM_KPFM InorganicCompound Ni81Fe19 NeodymiumMagnets Reduction cannabis TemperatureControllerAFM Strontium vertical_PFM Bacterium Blend semifluorinated alkane DentalProsthesis molecular_self_assembly PolycrystallineFerroelectricBCZT Defect
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Al2O3-doped CaMnO3
1% Al2O3-doped CaMnO3 on LaAlO3 (001) orientation substrate by pulsed laser deposition.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256