PrCurve Yeditepe_University Nanostructure graphene_hybrid ConductiveAFM LightEmiting HafniumDioxide atomic_steps Vanadate self-assembly EPFL Flake Phase CrossSection ImideMonomer hard_disk FrictionForce PvdfBead Formamidinium_lead_iodide Transparent TPU CrystalGrowing Hexacontane ThermalConductivity StyreneBeads Tungsten SrO LFM NCM\ PtfeMembrane block_copolymer 3-hexylthiophene BFO Steps ShenYang
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
AR Lens
Scanning Conditions
- System : FX40
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz for 40μm2, 1.5 Hz for 5μm2, 2μm2
- Scan Size : 40μm2, 5μm2, 2μm2
- Pixel Size : 2048×512 for 40μm2, 5μm2, 1024×256 for 2μm2
- Cantilever : OMCL-AC55TS (k=85N/m, f=1.6kHz)