PVAP3HT Spincast Magnetic Force Microscopy GlassTemp Aluminium_Oxide Self-assembledMonolayer Liquid C_AFM MESA structure Modulus hetero_structure Ni81Fe19 NusEce Annealing Ucl BiVO4 Hexylthiophene kelvin probe force microscopy MultiLayerCeramicCapacitor Ferroelectric SAM Hafnium_dioxide FM_KPFM Growth Varistor InLiquid PDMS Christmas Dr.JurekSadowski Fiber BCZT LifeScience Leakage Hafnia Ceramics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 Layers on SiO2
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256