BCZT hard_disk Blend Techcomp Defect Genetic CalciumHydroxyapatite GaP PatternedSapphireSubstrat Iron PolycrystallineFerroelectricBCZT LogAmplifier Molybdenum_disulfide Pzt Materials molecule LiftMode Worcester_Polytechnic_Institute Pore Reading Conductive AFM FM-KPFM Varistor pinpoint mode Ecoli BariumTitanate LiIonBattery Sapphire Annealing Organic PinPointMode PolyStylene Mechanical Terrace IRDetector
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256