ScanningKelvinProbeMicroscopy Epoxy suspended_graphene Mechinical SicMosfet ContactModeDot ScanningIon-ConductanceMicroscopy small_scan Polyaniline Conductance nanomechanical C36H74 Polytetrafluoroethylene Step Defect India CalciumHydroxyapatite silicon_carbide pulsed_laser_deposition Floppy Polydimethylsiloxane ThinFilm Chrome IcelandSpar Au111 DiffractiveOpticalElements LowDensityPolyethylene Tungsten piezoelectric force microscopy MagneticForce Hexatriacontane OrganicCompound non_contact Ferrite CuSubstrate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic Vortex Core (Ni-Fe alloy)
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm