Thermoplastic_polyurethane Force-distance PiezoelectricForceMicroscopy ContactMode ThinFilm FrictionForce SmalScan Roughness PatternedSapphireSubstrat silicon_carbide StrontiumTitanate Hydroxyapatite Non-ContactMode Treatment PVAP3HT Subhajjit Alloy Reduction SingleCrystal Optical IMT_Bucharest Protein NanoLithography self_assembly VerticalPFM Graphene SKPM AEAPDES Potential atomic_steps Implant conductive STO Materials phase_change
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
F14H20
Semifluorinated alkanes on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 05Hz, 1Hz
- Pixel Size: 1024 × 512, 512 x 256
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 05Hz, 1Hz
- Pixel Size: 1024 × 512, 512 x 256