amplitude_modulation DataStorage Mapping PrCurve AAO Boundary Reading Sperm Fiber UnivCollegeLondon HfO2 Chungnam_National_University semifluorinated_alkanes BiVO4 non_contact BreastCancerCell LiquidCell Annealing Sidewall lift_mode SPMLabs PinpointPFM UnivOfMaryland FastScan Vortex nanomechanical KPFM Bismuth PpLdpe atomic_steps PetruPoni_Institute oxide_layer Pinpoint PFM Scratch Neodymium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512