Annealing BiVO4 EFM flakes CHRYSALIS_INC atomic_steps hard_disk Silver Nanopattern ContactModeDot neodymium_magnets solar_cell ForceMapping Fujian HanyangUniv TCS block_copolymer KevlarFiber PFM NUS_Physics Hydroxyapatite Lanthanum_aluminate Formamidinium_lead_iodide Collagen PS_PVAC Lateral_Force_Microscopy Dimethicone AtomicLayer ElectroChemical MfmAmplitude PolycrystallineFerroelectricBCZT Boundary ElectroDeposition Regensburg Calcite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256