MeltingPoint UTEM neodymium_magnets StrontiumTitanate SKPM BismuthVanadate sputter Glass Austenite UnivCollegeLondon Polyurethane AtomicSteps BCZT VortexCore Polarization thermoplastic_elastomers ForceDistanceSpectroscopy Electrical&Electronics NCM Ferroelectric SiliconeOxide ForceMapping mfm_amplitude ElectrostaticForceMicroscopy Platinum SKKU Mechinical Thermoplastic_polyurethane Tin sulfide HDD Polystyrene SrTiO3 FastScan gallium_nitride SSRM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 1μm×1μm
- Scan Rate: 0.4Hz, 1Hz
- Pixel: 512×512, 512×512