CopperFoil CarbonNanotube LateralForceMicroscopy Epoxy BFO Korea Insulator LeakageCurrent Film F14H20 Piranha Biofilm Etch Growth Ceramic membrane C60H122 STO TriGlycineSulphate Neodymium SingleLayer ferromagnetic MechanicalProperties BlockCopolymer Phosphide bias_mode OpticalElement Friction LateralForce StainlessSteel RedBloodCell TiO2 C_AFM HACrystal Conductance
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG Moire
Scanning Conditions
- System: NX10
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128