Battery SRAM LFM PhaseTransition Permalloy kelvin probe force microscopy NiFe Trench fluorocarbon Bacteria Calcite NCM\ BTO #EC Regensburg Glass Tungsten Magnets lithography CntFilm dichalcogenide WWafer ForceVolumeMapping Conductivity DataStorage TyphimuriumBiofilm Mobile StainlessSteel OpticalModulator molecular_self_assembly Ca10(PO4)6(OH)2 PyroelectricDetector HexagonalBoronNitride LowDensityPolyethylene CuSubstrate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic Vortex Core (Ni-Fe alloy)
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm