Lateral polymeric_arrays LeakageCurrent Sulfur Electronics AAO temp_control P3HT ElectroDeposition piezoelectric force microscopy SurfaceOxidation PVA PVAC Zhi BaTiO3 Treatment EFMAmplitude Mechanical&nanotechnology Jason Hexylthiophene BloodCell Corrosion SingleCrystal Magnets Transparent PhaseTransition SrO ReflexLens organic_polymer Boron PatternedSapphireSubstrat GlassTemp Foil CalciumHydroxyapatite Global_Comm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Alkane Film (C60H122)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512