Varistor molecular_beam Barium_titanate Korea Mapping ThermalDetectors Pvdf IISCBangalore Plug Ito thermoplastic_elastomers Oxide FuelCell ShenYang LDPE Lanthanum_aluminate Device Regensburg dielectric trench PyroelectricDetector Vac HACrystal molecular_self_assembly Sphere PhthalocyaninePraseodymium PolyStylene NTU KevlarFiber TCS cannabinoid Croatia Pinpoint ULCA StrontiumTitanate light_emitting
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
C36H74
Layer of C36H74 alkane on HOPG.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256