ForceMapping Implant AEAPDES FastScan amplitude_modulation FrictionalForce PECurve thermal_conductivity BiasMode PDMS OpticalModulator DNA #EC Mapping OpticalElement atomic_steps Solar Cobalt-dopedIronOxide TyphimuriumBiofilm Yttria_stabilized_Zirconia Piezoresponse NTU MembraneFilter KelvinProbeForceMicroscopy Biology AAO thermoplastic_elastomers Alloy ElectroChemical CopperFoil AIN Resistance Sio2 Aluminum Korea
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cutting Graphene
Scanning Conditions
- System : FX40
- Scan Mode: Contact after lithography
- Scan Rate : 0.7 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)
- Lithography condition : Force 500 nN, writing speed 0.1μm/s, AC bias 10 V @ 40kHz