Oxide FastScan Optoelectronic Al2O3 LateralForce Logo molecular_self_assembly domain_switching Non-ContactMode ScanningTunnelingMicroscopy ScanningKelvinProbeMicroscopy Magnetic Conductive AFM Vacuum Trench temp_control Semiconductor ContactModeDots aluminum_nitride Chromium FrequencyModulation TransitionMetal Indium_tin_oxide GlassTemp StainlessSteel Mosfet ULCA F14H20 MultiLayerCeramicCapacitor India MfmPhase Conductance Deposition Scratch Graphite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcium Hydroxyapatite Crystal growing
HA crystal grows according to the annealing time. From 24hrs, the crystal becomes clearly.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256