Battery IcelandSpar IVSpectroscopy BTO LiIonBattery PatternedSapphireSubstrat Pyroelectric TungstenThinFilmDeposition Wildtype Hafnia Modulus NeodymiumMagnets LiBattery Austenite CarbonNanotube Moire Fe_film Biology Etch CalciumHydroxyapatite CastIron SFAs Domain FrictionalForce Blend Heating MLCC FrequencyModulation Annealed DentalProsthesis Tungsten DomainSwitching molecular_self_assembly Indium_tin_oxide Butterfly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic patterned array
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128