MetalCompound GlassTemp Sidewall silicon_oxide Glass Gold DOE non_contact Holes block_copolymer Photovoltaics Piezoresponse OrganicCompound Pattern LateralPFM PVA STO Austenite Varistor Hair Solution contact Scratch Stiffness temperature controller AFM Logo ForceDistanceSpectroscopy Hexylthiophene Tin sulfide WWafer Magnetic Hafnia Current AmplitudeModulation CNT
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CNT Film
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 45μm×45μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Sample Bias: +0.3V
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 45μm×45μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Sample Bias: +0.3V