Pores Roughness Conductivity Vinylpyridine IVSpectroscopy SrTiO3 STO Hexylthiophene CeNSE_IISc Optic StrontiuTitanate Molybdenum TemperatureControllerAFM Self-assembledMonolayer OxideLayer MonoLayer temp VinylAlcohol Kevlar AM_SKPM SingleLayer EFMAmplitude EPFL Varistor NiFe PolyStylene PhaseTransition PolycrystallineFerroelectricBCZT piezoelectric force microscopy Nanofiber Sio2 C_AFM DeoxyribonucleicAcid Korea ThermalConductivity
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li ion battery electrode
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm
- Scan Rate: 1Hz
- Pixel: 4096×2048