Hysteresys ItoGlass ElectroChemical BariumTitanate Flake ScanningSpreadingResistanceMicroscopy polyvinyl acetate YttriaStabilizedZirconia Hexacontane MfmAmplitude Force-distance Ucl food organic_polymer Ceramic Tungsten thermal_conductivity CuFoil FrictionForce PinpointNanomechanicalMode Dopped lithography Display CNT BismuthFerrite Bio fluoroaalkane MultiLayerCeramicCapacitor Sic Hexylthiophene Techcomp BismuthVanadate Sidewall NanoLithography KevlarFiber
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V