Aluminium_Oxide MolecularSelfAssembly Ptfe 3-hexylthiophene atomic_layer MfmPhase thermoplastic_elastomers food KelvinProbeForceMicroscopy Sphere FrequencyModulation Pvdf GlassTemp Grain FailureAnalysis Growth MBE AM-KPFM Optoelectronic light_emitting BismuthVanadate Indent FAFailureAnlaysis MESA structure Dimethicone PatternedSapphireSubstrat TipBiasMode molecular_beam Vanadate Self-assembledMonolayer Hexacontane mfm_amplitude HumanHair Croatia TyphimuriumBiofilm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Composite Barium Titanate
PFM Quad color is overlaid on 3D surface morphology.
Scanning Conditions
- System: NX10
- Scan Mode: PFM
- Cantilever: PPP-ContScPt (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 256 × 256
- Scan Mode: PFM
- Cantilever: PPP-ContScPt (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 256 × 256