heterojunctions Switching molecular_self_assembly MfmPhase MagneticArray ThermalConductivity hard_disk_media Hexylthiophene semifluorinated_alkane semifluorinated alkane OpticalElement SurfaceChange SmalScan Beads SingleCrystal Magnetic Force Microscopy HardDisk Polyethylene Hafnium_dioxide FloppyDisk BiVO4 thermal_conductivity Collagen Dimethicone InorganicCompound PtfeMembrane Gong lithography HBN SThM FAFailureAnlaysis Optic PinpointNanomechanicalMode Chungnam_National_University Piezo
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
STO(SrTiO3), Annealed LAO(LaAlO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm, 5μm×5μm
- Scan Rate: 0.8Hz, .9Hz
- Pixel: 512×512, 256×256