Hydroxyapatite Potential blended polymers Ceramic Tungsten_disulfide Organic Wafer Morphology plastics Reduction Nanopattern MfmPhase SolarCell IISCBangalore CVD Ananth ThermalDetectors VortexCore CarbonNanotube DataStorage NeodymiumMagnets Pores Heating NUSNNI cooling BlockCopolymer molecular_self_assembly Change Domain Blood IIT-chennai Heat SrO Temperature SiWafer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256